McCright, R. D.; Frey, W. F.; Tardiff, G. E.
·
Geothermal Resources Council Transactions
·
1980
·Corrosion; Steel
Coupons of eight different carbon and chrome-moly alloy steels were exposed to high temperature, high salinity wellhead brine blow at a geothermal well in the Salton Sea Geothermal Field for periods of up to six months. The corrosion rate and corrosion attack …
View paper: Localized Corrosion of Steels in Geothermal Steam/Brine Mixtures
Download unavailable
-
Grassiani, M.
·
Geothermal Resources Council Transactions
·
2004
·Power Plants; Corrosion; Pitting; Austenitic Stainless Steel
View paper: Stainless Steel Corrosion in Geothermal Condensing Steam
Download unavailable
-
J.J.Blangé, A.Reinicke
·
World Geothermal Congress
·
2026
·Advances in Drilling Technologies & Data - Part 1
… years, the start-up Canopus developed the Directional Steel Shot Drilling (DSSD) technology. DSSD is a unique combination of the latest Polycrystalline Diamond Compact (PDC) bit technology and steel shot erosion. The hybrid PDC-steel shot erosion …
View paper: Fast Hole Making while Steering with Directional Steel Shot Drilling: Technology Overview and Field Performance
PDF: Fast Hole Making while Steering with Directional Steel Shot Drilling: Technology Overview and Field Performance
-
Natsuki Hirabayashi
·
World Geothermal Congress
·
2026
·Poster
… piping. We implemented corrosion tests of stainless steel in acidic fluids in subcritical regions. Corrosion tests for type 430 stainless steel were conducted in acidic fluid with high chloride ions at 250 ℃. The stainless steel is a general-purpose …
View paper: Corrosion of Type 430 Stainless Steel at 250 ℃ in Acidic Fluids
PDF: Corrosion of Type 430 Stainless Steel at 250 ℃ in Acidic Fluids (1054KB)
-
Sukanya Hägg Mameng, Cauê Corrêa da Silva and Daniel Svedberg
·
Der Geothermiekongress
·
2025
… aims to provide insights into various grades of stainless steel that are particularly suitable for geothermal energy applications, with a focus on their corrosion resistance in brine. For well construction it is paramount to assess the influence of design …
View paper: Resistance of stainless steels to crevice corrosion, SCC and corrosion of welded joints
PDF: Resistance of stainless steels to crevice corrosion, SCC and corrosion of welded joints (592 KB)
-
S. Ghazio, K. Lichti, M. Sato, K. Osato, N. Yanagisawa, K. Sakura
·
New Zealand Geothermal Workshop
·
2023
·Session 5.2 - SCALING & CORROSION
… evaluation of the corrosion behavior of K55 and new casing steels in an acid steam condensate derived from high temperature HCl gas contaminated steam condensing at atmospheric pressure and a temperature of the order of 97 °C. A Steam Condensate Test rig was …
View paper: Laboratory HCl acid condensate testing of geothermal casing steels
PDF: Laboratory HCl acid condensate testing of geothermal casing steels (425KB)
-
Knebel, Marcel (1); Blangé, Jan-Jette (2); Reinicke, Andreas (3); Zikovic, Vedran (4); Lassnig, Erich (5); Schenk, Beni (6); Sikirica, Mile (1); Kesler, Scott (7); Dwars, Sicco (8); Martin, Francois (9); Degener, Floris (1); van Bergen, Frank (3)
·
Der Geothermiekongress
·
2023
Directional Steel Shot Drilling" (DSSD), a novel directional drilling technology developed by Canopus Drilling Solutions B.V., offers an innovative solution to enhance the productivity and cost-effectiveness of geothermal drilling. Conventional drilling often …
View paper: Novel "Directional Steel Shot Drilling“ – technology from Canopus Drilling Solutions B.V. – Preparation and results of an extensive lab and field test
PDF: Novel "Directional Steel Shot Drilling“ – technology from Canopus Drilling Solutions B.V. – Preparation and results of an extensive lab and field test (1321 KB)
-
Norio YANAGISAWA, Masatake SATO, Kazumi OSATO, Yu YAMAMOTO, Keith LICHTI, Bruce MOUNTAIN, Lucjan SAJKOWSKI
·
Stanford Geothermal Workshop
·
2021
·Emerging Technology
… acid, were used. Three types of specimens, TN125Cr13U steel, TN110Cr13S steel, and 17Cr steel were used, and the tests were conducted to a maximum flow rate of 10 L/ min for about 1,3 and 8 days. The corrosion rate was calculated from the change in …
View paper: Material Corrosion Test for Developing Cr Casing Steel at High Temperature Acid Condition
PDF: Material Corrosion Test for Developing Cr Casing Steel at High Temperature Acid Condition (710 KB)
-
Norio YANAGISAWA, Masatake SATO, Kazumi OSATO, Yu YAMAMOTO, Koji SAKURA, Keith LICHTI, Bruce MOUNTAIN, Lucjan SAJKOWSKI
·
Stanford Geothermal Workshop
·
2020
·General
… acid, were performed. Three types of specimens, TN125Cr13U steel, TN110Cr13S steel, and 17Cr steel, were used, and a test was conducted at a maximum flow rate of 200 L / min for about 5 hours. The corrosion rate was calculated from 1) the total dissolved …
View paper: Corrosion Test of Casing Steel at High Temperature Acid Condition
PDF: Corrosion Test of Casing Steel at High Temperature Acid Condition (565 KB)
-
Francois ROPITAL, Jean KITTEL
·
World Geothermal Congress
·
2020
·Corrosion and Scaling
… lead to severe corrosion damages for carbon and stainless steels geothermal equipment. If supercritical CO2 can occur naturally in a reservoir, it is also a promising heat transmission fluid for enhanced geothermal systems (EGS). The quantity of water …
View paper: Corrosion Evaluation of Steels Under Geothermal CO2 Supercritical Conditions
PDF: Corrosion Evaluation of Steels Under Geothermal CO2 Supercritical Conditions (583 KB)
-
Masatake SATO, Kaichiro KASAI, Kazumi OSATO, Norio YANAGISAWA, Yu YAMAMOTO, Toshihiko FUKUI, Koji SAKURA, Bruce MOUNTAIN, Soroor GHAZIOF, Keith LICHTI
·
World Geothermal Congress
·
2020
·Corrosion and Scaling
Casing steels of geothermal wells are exposed to high temperature brine and brine of especially low pH, which are capable of causing serious corrosion. The object of this work was to identify cost-effective casing materials under several acidic geothermal …
View paper: Laboratory Corrosion Testing of Casing Steels in Acidic Brine and Field Testing at Kakkonda Geothermal Field, Japan
PDF: Laboratory Corrosion Testing of Casing Steels in Acidic Brine and Field Testing at Kakkonda Geothermal Field, Japan (1491 KB)
-
Norio YANAGISAWA, Yoshio MASUDA, Masatake SATO, Kaichiro KASAI, Kazumi OSATO, Toshihiko FUKUI, Koji SAKURA, Keith LICHTI
·
World Geothermal Congress
·
2020
·Corrosion and Scaling
… test was carried out using 30 mm size test piece of carbon steel, low metal alloy and stainless steel settled in the small loop flow system. The test condition was pH 3.8,165 degreeC and 4.5L/min flow rate condition. And to estimate the corrosion rate in …
View paper: Corrosion Testing of Casing Steels in Acidic Two Phase Production Fluid and the Field Testing at Yanaizu-Nishiyama Geothermal Field, Japan
PDF: Corrosion Testing of Casing Steels in Acidic Two Phase Production Fluid and the Field Testing at Yanaizu-Nishiyama Geothermal Field, Japan (806 KB)
-
S. Ghaziof, R. Dudley, R. Julian, M. Ko and K. Lichti
·
New Zealand Geothermal Workshop
·
2017
·Session 3.2 Scaling
Corrosion of carbon and low alloy steels in H2S containing geothermal two phase fluids, separated steam and superheated steam has long been known to be controlled by the formation of adherent and continuous iron sulphide and iron oxide corrosion products that …
View paper: H2S Corrosion of Carbon Steel in Geothermal Fluids
PDF: H2S Corrosion of Carbon Steel in Geothermal Fluids (698KB)
-
Amela KESEROVIC, Ralph BÄSSLER
·
World Geothermal Congress
·
2015
·Corrosion and Scaling
… different factors on the corrosion performance of carbon steel, the most widely used engineering material, and its integrity. This way the probability of the material failure would be minimized and a safer operating window of power plants would be …
View paper: Geothermal Systems of Indonesia – Influence of Different Factors on the Corrosion Performance of Carbon Steel API Q125
PDF: Geothermal Systems of Indonesia – Influence of Different Factors on the Corrosion Performance of Carbon Steel API Q125 (260 KB)
-
Keith LICHTI, Lilly WALLIS, Monika KO, John KENNEDY
·
World Geothermal Congress
·
2015
·Corrosion and Scaling
Carbon steel has been observed to experience accelerated corrosion in some pH adjusted geothermal brines. The damage mechanisms observed in service have included; localised under-film corrosion, galvanic corrosion and erosion corrosion. The magnitude of these …
View paper: Kinetics of Galvanic Corrosion of Carbon Steel to Arsenic and Antimony Couples
PDF: Kinetics of Galvanic Corrosion of Carbon Steel to Arsenic and Antimony Couples (2347 KB)
-
Geir THOROLFSSON and Asbjorn EINARSSON
·
World Geothermal Congress
·
2015
·Corrosion and Scaling
… fluid is of seawater origin. Up to 2006 cracking of mild steel steam pipes occurred occasionally, generally in the vicinity of welding seams. However, after nine months operation of the Reykjanes Power Plant the cracking problem increased dramatically. …
View paper: The Influence of the Manganese Content of Mild Steel on the Rate of Crack Formation in Geothermal Steam Pipes at the Reykjanes Power Plant in Iceland
PDF: The Influence of the Manganese Content of Mild Steel on the Rate of Crack Formation in Geothermal Steam Pipes at the Reykjanes Power Plant in Iceland (1127 KB)
-
Sakanaka, Yoshikazu
·
Geothermal Resources Council Transactions
·
2007
·Turbines; Stress corrosion cracking; Chromium
… the reliability of geothermal turbine further, 12%Cr steel has been developed and actually applied for both rotor forging and welding material for refurbishment. In this paper, the result of verification study of 12%Cr steel and the weld repair by …
View paper: Application of 12%Cr Steel for Geothermal Turbine Rotor
Download unavailable
-
Keith A. Lichti, David M. Firth and Annette D. Karstensen
·
World Geothermal Congress
·
2005
·20. Corrosion and Scaling
Typically, low strength steels and annealed stainless steels are specified for geothermal energy applications because of the risk of Sulfide induced Stress Corrosion Cracking (SSCC) and Hydrogen Induced Cracking (HIC) in the presence of H2S containing fluids. …
View paper: Hydrogen Induced Cracking of Low Strength Steels in Geothermal Fluids
PDF: Hydrogen Induced Cracking of Low Strength Steels in Geothermal Fluids (687KB)
-
Mohamed Amalhay, Catherine Cotiche and Ioannis Ignatiadis
·
World Geothermal Congress
·
1995
·SECTION 11 - Corrosion and Scaling
… the in the difficulties in the of corrosion of carbon steel well casings, scaling and due essentially to the of the fluids In ordcr to optimize anticorrosion in wells. various corrosion inhibitors were tested Using techniques (monitnring circuit …
View paper: Study of the Electrochemical Behaviour of a Carbon Steel in a Real and Treated Geothermal Environment
PDF: Study of the Electrochemical Behaviour of a Carbon Steel in a Real and Treated Geothermal Environment
-
Sugama, Toshifumi; Gill, Simerjeet K.; Muraca, Amanda; Pyatina, Tatiana
·
Geothermal Resources Council Transactions
·
2013
·Equipment design; Cementing; Corrosion; HDR/EGS
View paper: Corrosion-Resistant Foamed Cements for Carbon Steels in Enhanced Geothermal Systems
Download unavailable
-
Hernandez Morales, David
·
Geothermal Resources Council Transactions
·
2003
·Drilling; Corrosion
View paper: Effect of Temperature on the Yield Strength of Steel
Download unavailable
-
Sugama, Toshifumi; Gawlik, Keith; Sullivan, Bob
·
Geothermal Resources Council Transactions
·
2006
·Geofluids; corrosion; Scaling; heat exchangers; carbon steel
… brine, the new coating, applied to aluminum fins and steel coupons, showed significant improvements in corrosion and scaling resistance over previous coatings that did not include cerium oxide doping, and also showed that corrosion resistance improved …
View paper: Field Testing and Analysis of Air-Cooled Condenser Components Coated with Cerium Oxide-Doped PAAMPS Polymer Nanocomposite Material
Download unavailable
-
Gawlik, Keith; Sugama, Toshifumi; Webster, Ronald; Reams, Walter
·
Geothermal Resources Council Transactions
·
2000
·Scaling; Corrosion; Heat Exchangers; Carbon Steel
View paper: Development and Field Testing of Polymer Heat Exchanger Tube Coatings
Download unavailable
-
Harry Tookey
·
World Geothermal Congress
·
2026
·Poster
Carbon steel within geothermal systems can be impacted by corrosion due to carbon dioxide (CO2) dissolved in the fluid. Chemical inhibitors are typically used to mitigate the corrosion. However, many corrosion inhibitors are toxic and environmentally harmful. …
View paper: Challenges for Green Inhibitor Development for Geothermal Applications
PDF: Challenges for Green Inhibitor Development for Geothermal Applications (3821KB)
-
Anastasia STOLJAROVA, Ralph BAESSLER, Simona REGENSPURG
·
World Geothermal Congress
·
2020
·Corrosion and Scaling
… with the evaluation of the corrosion behavior of carbon steel and corrosion resistant alloys in copper and/or lead containing artificial geothermal water, simulating the conditions in the Northern German Basin. The behavior of these materials in an …
View paper: Influence of Precipitating Brine Components on Materials Selection for Geothermal Applications
PDF: Influence of Precipitating Brine Components on Materials Selection for Geothermal Applications (1096 KB)