Tatiana PYATINA, Toshifumi SUGAMA
·
World Geothermal Congress
·
2020
·Drilling and Completion Technology
… Cement chemistry modified with pozzolanic materials, slag, chemical and hydraulic calcium-aluminate cement-based blends and combinations of different types of fly ash at early ages (up to 28 days of the initial curing) after repeated compressive damage …
View paper: Self-healing, Re-adhering and Carbon-Steel Corrosion-Mitigating Inorganic Cement Composites for Geothermal Wells at 300degC
PDF: Self-healing, Re-adhering and Carbon-Steel Corrosion-Mitigating Inorganic Cement Composites for Geothermal Wells at 300degC (1285 KB)
-
Sugama, Toshifumi; Pyatina, Tatiana
·
Geothermal Resources Council Transactions
·
2014
·HDR/EGS; Fractures; Cementing; Drilling; Equipment design; L
… self-degradation of sodium metasilicate (SMS)-activated slag/Class C fly ash cement containing PVA fiber-bridging additive. The cement is used as temporary sealer for fractures in Enhanced Geothermal System (EGS) wells under a hydrothermal environment at …
View paper: Utilization of PVA Flakes in Promoting Self-Degradation of Temporary Cementitious Fracture Sealing Material
Download unavailable
-
Baris ALP and Serhat AKIN
·
Stanford Geothermal Workshop
·
2013
·Emerging Technology
… temperatures of 230 ºF. Ground granulated blast furnace slag (GGBFS) has a Ca/Si ratio lower than 1 and thus silica does not need to be added to cement. The hydration of GGBFS blended cement pastes are improved at elevated temperatures that has vital …
View paper: Utilization of Supplementary Cementitious Materials in Geothermal Well Cementing
PDF: Utilization of Supplementary Cementitious Materials in Geothermal Well Cementing (1403 K)
-
Sugama, Toshifumi; Butcher, Thomas; Brothers, Lance; Bour, Daniel
·
Geothermal Resources Council Transactions
·
2011
·HDR/EGS; Drilling; Cementing; Lost circulation; Temporary fr
Self-degradable slag (S)/Class C or F fly ash blend pozzolana cements were formulated, assuming that they might serve well as alternative temporary fracture sealers in Enhanced Geothermal System (EGS) wells operating at temperatures of ? 200°C. The candidate …
View paper: Temporary Cementitious Sealing Materials
Download unavailable
-
Denduluri, Veerabhadra S; Genedy, Moneeb; Juenger, Maria; McDonald, Mike; van Oort, Eric
·
Geothermal Resources Council Transactions
·
2022
·Drilling; Lost circulation; Cementing; Polymers
View paper: Using Geopolymers as a Sustainable Alternative Cementing Solution for Long-Term Zonal Isolation and Lost Circulation Challenges in Deep Geothermal Wells
Download unavailable
-
Carl Bigley, Ian Brown, Bede Geoghegan, Andreas Brandl
·
World Geothermal Congress
·
2010
·21. Drilling and Completion Technology
The shortcomings of regular grades of Portland cements used in service temperature environments above 110°C are well known. The metastable Calcium Silicate Hydrate reaction products recrystallise as generally denser, lower volume forms such as α-C2SH, …
View paper: A New Portland Cement Derived Composite Binder for Use in Geothermal Wells
PDF: A New Portland Cement Derived Composite Binder for Use in Geothermal Wells (264KB)