I. THORBJORNSSON, B.C KROGH, G.S.KALDAL, G.RÖRVIK, S.S. JONSSON, L. GUDMUNDSSON, F. OSKARSSON
·
World Geothermal Congress
·
2020
·Corrosion and Scaling
Selection of materials for high-temperature geothermal wells follows oil and gas (O&G) standards and recommendations and the same applies for wellhead design, well design and drilling. Geothermal wells differ from O&G wells with higher temperatures and …
View paper: Corrosion Testing in Direct Geothermal Steam of Cladded and Stand Alone Materials at 210°C and 450°C
PDF: Corrosion Testing in Direct Geothermal Steam of Cladded and Stand Alone Materials at 210°C and 450°C (1689 KB)
-
N. Yanagisawa, Y. Masuda, M. Sato, K. Kasai, K. Osato, K. Sakura
·
New Zealand Geothermal Workshop
·
2019
·Session 2.3 – Silica & Corrosion 1
… in November 2017. And we compared the results with the material corrosion prediction equation using a Cr equivalent amount, as proposed by Kurata et al. (1992). In the field test, the temperature was 145 ° C, the initial base case pH was 5.15, and then …
View paper: The material corrosion test on pH adjustment condition by acid at geothermal field in Japan
PDF: The material corrosion test on pH adjustment condition by acid at geothermal field in Japan (271KB)
-
Tevfik Kaya, Pelin Hoshan
·
World Geothermal Congress
·
2005
·20. Corrosion and Scaling
… have occurred regarding the corrosion and the usage of the materials that are influence the effectiveness and the quality of the service. The knowledge of the characteristics of the geothermal fluid partly leading to the breakdown of the equipment used for …
View paper: Corrosion and Material Selection for Geothermal Systems
PDF: Corrosion and Material Selection for Geothermal Systems (65KB)
-
Tacchino, Gian Carlo
·
Geothermal Resources Council Transactions
·
1983
·Corrosion; Brine chemistry; Turbines; Condensers; Durability
… etc. We have accumulated considerable experience on materials behavior that lead us to the solicitation of the martensitic 13cr rotors, AISI 316 condenser, etc. These materials are presently used for the equipment that ANSALDO is supplying for a …
View paper: Corrosion in Geothermal Plant: Choice and Use of Special Materials
Download unavailable
-
Norio YANAGISAWA, Masatake SATO, Kazumi OSATO, Yu YAMAMOTO, Keith LICHTI, Bruce MOUNTAIN, Lucjan SAJKOWSKI
·
Stanford Geothermal Workshop
·
2021
·Emerging Technology
… for high-temperature acidic hot water, we carried out the material corrosion tests using a flow-through autoclave at GNS Science, New Zealand. A test piece, having a diameter of 8 mm and a length of 13 mm, was isolated with zirconia beads inside a pressure …
View paper: Material Corrosion Test for Developing Cr Casing Steel at High Temperature Acid Condition
PDF: Material Corrosion Test for Developing Cr Casing Steel at High Temperature Acid Condition (710 KB)
-
Norio YANAGISAWA, Yoshio MASUDA, Hiroshi ASANUMA
·
World Geothermal Congress
·
2020
·Advanced Technology (Magma, Geopressure, etc.)
The material corrosion is one of issue for the development of super-critical geothermal resources. To solve the problems, we tried to estimate the behavior of corrosive fluid of the several developing stage including drilling, production using Slveq-Chim by …
View paper: Survey of the Casing Material Corrosion Problem for Supercritical Geothermal Development
PDF: Survey of the Casing Material Corrosion Problem for Supercritical Geothermal Development (263 KB)
-
N. Yanagisawa,Y. Masuda, K. Osato, M. Sato, K. Kasai, K. Sakura, T. Fukui, M. Akahori and K. Lichti
·
New Zealand Geothermal Workshop
·
2017
·Session 3.2 Scaling
We carried out the material corrosion in acidic fluid under two-phase conditions at Yanaizu-Nishiyama, Okuaizu geothermal power plant using small loop test system in February of 2017. We carried out several corrosion tests, 1 day, 4 days and 15 days testing …
View paper: THE MATERIAL CORROSION TEST USING LOOP SYSTEM UNDER ACIDIC CONDITION AT GEOTHERMAL FIELD IN JAPAN
PDF: THE MATERIAL CORROSION TEST USING LOOP SYSTEM UNDER ACIDIC CONDITION AT GEOTHERMAL FIELD IN JAPAN (502KB)
-
Novianti EKASARI, Bonar T.H. MARBUN
·
World Geothermal Congress
·
2015
·Drilling and Completion Technology
… modelling. This study has been implemented for selecting materials casing in well conditions similar to well “A” in a geothermal field in Indonesia. Based on this study, it is known that the corrosion rate equation by Kurata et al cannot be applied in …
View paper: Integrated Analysis of Optimizing Casing Materials Selection of Geothermal Well by Using a Model for Calculating Corrosion Rates
PDF: Integrated Analysis of Optimizing Casing Materials Selection of Geothermal Well by Using a Model for Calculating Corrosion Rates (1008 KB)
-
N. Yanagisawa, M. Sato, K. Osato, Y. Yamamoto, K. Lichti, B. Mountain, and L. Sajkowski
·
New Zealand Geothermal Workshop
·
2021
·Session 5.3 - Casing and Corrosion
… for high-temperature acidic hot fluid, we carried out the material corrosion tests using a flow-through autoclave at GNS Science, New Zealand. A test piece, having a diameter of 8 mm and a length of 13 mm, was isolated with zirconia beads inside a pressure …
View paper: CORROSION RATE ESTIMATION OF Cr CASING STEELS AT HIGH TEMPERATURE ACID CONDITIONS
PDF: CORROSION RATE ESTIMATION OF Cr CASING STEELS AT HIGH TEMPERATURE ACID CONDITIONS (729KB)
-
Norio YANAGISAWA, Yoshio MASUDA, Masatake SATO, Kaichiro KASAI, Kazumi OSATO, Toshihiko FUKUI, Koji SAKURA, Keith LICHTI
·
World Geothermal Congress
·
2020
·Corrosion and Scaling
The material corrosion test in acidic fluid and two-phase condition was carried out at Yanaizu-Nishiyama geothermal field. The test was carried out using 30 mm size test piece of carbon steel, low metal alloy and stainless steel settled in the small loop flow …
View paper: Corrosion Testing of Casing Steels in Acidic Two Phase Production Fluid and the Field Testing at Yanaizu-Nishiyama Geothermal Field, Japan
PDF: Corrosion Testing of Casing Steels in Acidic Two Phase Production Fluid and the Field Testing at Yanaizu-Nishiyama Geothermal Field, Japan (806 KB)
-
Blakely, Michael; Olivas, Jose
·
Geothermal Resources Council Transactions
·
2010
·Corrosion; Welding
… are unavoidable. These factors are driving engineering material selection for many components, including piping and pressure vessels, to higher alloys of stainless steel, nickel based alloys and titanium. The costs of these materials can be significant …
View paper: Explosion Welded Materials for Geothermal Appliations
Download unavailable
-
Amend, Bill
·
Geothermal Resources Council Transactions
·
2009
·Corrosion; Stress corrosion cracking
Selection of cost effective materials of construction for geothermal applications requires that designers and operators recognize and understand the mechanisms by which candidate materials can degrade in the various geothermal fluids. Once the applicable …
View paper: Considerations in the Testing and Selection of Materials for Corrosive Geothermal Environments
Download unavailable
-
Gallup, Darrell L.
·
Geothermal Resources Council Transactions
·
2002
·Corrosion; Oxygen; Cooling Towers; Inhibition; Materials of
View paper: Differential Oxygen Cell Corrosion in Aerated Condensate of Brine Re-Injection Wells
Download unavailable
-
Yoshiaki Kurata, Norio Sanada, Hiroshi Nanjo, Jun Ikeuchi and Keith A. Lichti
·
World Geothermal Congress
·
1995
·SECTION 11 - Corrosion and Scaling
Field testing of materials at White Island was undertaken to asses the corrosion performance of metals and alloys under the severe corrosive conditions encountered in geothermal volcanic environments. Metallic materials were tested in six different types of …
View paper: Material Damage in a Volcanic Environment
PDF: Material Damage in a Volcanic Environment
-
Conover, Marshall F.; Ellis, Peter F.
·
Geothermal Resources Council Transactions
·
1979
·Corrosion; Liquid dominated reservoirs; Power plant design a
A second Edition Handbook on Material Selection Guidelines for Geothermal Energy Systems is in final preparation. This DOE funded effort emphasizes that the most important difference between traditional steam systems and those that utilize geothermal fluids …
View paper: Materials Selection Guidelines for Geothermal Energy Systems
Download unavailable
-
Toney, S.; Tuncel, O.; Cohen, M.
·
Geothermal Resources Council Transactions
·
1982
·Turbines; Durability testing; Corrosion
A considerable number of onsite material test programs have been conducted at different geothermal sites to provide a database which permits characterization of materials used, or considered potentially useful, for geothermal turbine applications. These …
View paper: Geothermal Turbines -- Materials Evaluation and Design Aspects
Download unavailable
-
Thain, I. A.; Stacey, R. E.; Nicholson, D. J.
·
Geothermal Resources Council Transactions
·
1981
·Corrosion; Pipelines
… pressure. However, these remedies appear to have caused corrosion in the HP steam liens to the extent of seriously threatening their pressure integrity. Extensive experimentation and studies were carried out before a cure was obtained. This report details …
View paper: Zero Solids Condensate Corrosion in Steam Pipes at Wairakei
Download unavailable
-
Sigrun N. Karlsdottir, Gifty Oppong Boakye, Daniel Agbonluai Ijegbai, María Y. Thrainsdottir, Erlend
·
World Geothermal Congress
·
2026
… increased corrosion and erosion-corrosion of well casing materials. To ensure the durability of casing materials, corrosion testing under harsh conditions—high temperature, high pressure, and corrosive gases—is essential. This study reports results on the …
View paper: High Temperature and High Pressure Testing of Well Casing Materials for Superhot Geothermal Wells
PDF: High Temperature and High Pressure Testing of Well Casing Materials for Superhot Geothermal Wells
-
Norio YANAGISAWA, Masatake SATO, Koji SAKURA
·
Stanford Geothermal Workshop
·
2023
·Production Engineering
… (acidic hot water version)" that can consider the optimal materials for power plant construction when the hot water for geothermal power generation is found to be acidic. If the geothermal resource is acidic hot water, the corrosion and damage to the power …
View paper: Development of Corrosion Risk Evaluation System in Acidic Geothermal System
PDF: Development of Corrosion Risk Evaluation System in Acidic Geothermal System (1162 KB)
-
Norio YANAGISAWA, Masatake SATO, Kazumi OSATO, Yu YAMAMOTO, Koji SAKURA, Keith LICHTI, Bruce MOUNTAIN, Lucjan SAJKOWSKI
·
Stanford Geothermal Workshop
·
2020
·General
… hot water that has not been used so far by evaluating the material corrosion characteristics of high-temperature acidic hot water at about 300 ° C and above pH3. As one of the evaluation methods, a material corrosion test using a flow type autoclave of New …
View paper: Corrosion Test of Casing Steel at High Temperature Acid Condition
PDF: Corrosion Test of Casing Steel at High Temperature Acid Condition (565 KB)
-
Tatiana PYATINA, Toshifumi SUGAMA
·
World Geothermal Congress
·
2020
·Drilling and Completion Technology
… thermal shock and acid resistance of various cementitious materials under high-temperature (300°C) hydrothermal conditions. Experimental results are presented for formulations based on Ordinary Portland Cement chemistry modified with pozzolanic materials, …
View paper: Self-healing, Re-adhering and Carbon-Steel Corrosion-Mitigating Inorganic Cement Composites for Geothermal Wells at 300degC
PDF: Self-healing, Re-adhering and Carbon-Steel Corrosion-Mitigating Inorganic Cement Composites for Geothermal Wells at 300degC (1285 KB)
-
H. Heinzel, B. Habib, M. Karpenko
·
New Zealand Geothermal Workshop
·
2016
·1.2
… of the brine, the process conditions and the selected material. Test results obtained under idealized conditions in laboratory set-ups are not always a true indicator for the performance of the material under operational conditions and need to be …
View paper: Field-Based Material Test Rig for Geothermal Orc Plant Components
PDF: Field-Based Material Test Rig for Geothermal Orc Plant Components (528KB)
-
H. Heinzel, B. Habib, M. Karpenko
·
New Zealand Geothermal Workshop
·
2015
·Session 1B: Above Ground
… of the brine, the process conditions and the selected material. In the context of material selection, the guiding question is: ‘What material performs best for any given application in the Above Ground Geothermal and Allied Technologies (AGGAT) …
View paper: DEVELOPMENT OF A FIELD-BASED MATERIALS TEST-RIG
PDF: DEVELOPMENT OF A FIELD-BASED MATERIALS TEST-RIG (169KB)
-
Villa, Ruperto R., Jr.; Paraon, June Rizza V.; Lichti, Keith A.
·
Geothermal Resources Council Transactions
·
2002
·Corrosion; Geothermal Condensate Fluids
View paper: Effect of pH Elevation by NaOH Dosing on the Corrosion Potential of Steam Condensate Fluids from the Upper Mahiao Power Station, Leyte, Philippines
Download unavailable
-
Norio Sanada, Yoshiaki Kurata, Hiroshi Nanjo, Hyun-soo Kim, Jun Ikeuchi and Keith A Lichti
·
World Geothermal Congress
·
2000
·Drilling and Completion Technology
The IEA Deep Geothermal Initiative, Subtask C on materials has been progressed by surveys of deep geothermal well experience and research results. This work revealed that the chemistry of deep geothermal fluids is expected to be more acidic than is …
View paper: IEA Deep Geothermal Resources Subtask C: Materials, Progress with a Database for Materials Performance in Deep and Acidic Geothermal Wells
PDF: IEA Deep Geothermal Resources Subtask C: Materials, Progress with a Database for Materials Performance in Deep and Acidic Geothermal Wells (311 B)